Printing process
The printing staff first obtains the corresponding screen, ink, and adhesive materials according to the production subpena and process card requirements, and performs the mutual inspection work. Specifically, the printing personnel include: 1) The received screen printing plate, whether the ink meets production subpena or process card requirements. 2 screen quality meets the quality requirements for printing; 3 check the surface quality of the edges of adhesive materials. After the inspection is correct, fix the screen and fix the net distance, and then use the positioning material for positioning. In this case, the position of the printing pattern must be determined according to the positioning frame. The three positioning pieces are located at 1/3 of each positioning edge. The size of the positioning piece is specified as 1cm x 2cm, and the position of the positioning piece at the edge of the adhesive material is marked when the original positioning is performed.
The first piece of paper is printed before the plate is printed. After the first piece of monochrome is printed, it must be confirmed by the quality inspector. Sign the "Agree to Print" on the color sample of the first product and sign it; The contrast check, found abnormal, to do appropriate adjustments, such as adding thinner, adjusting the angle of the blade, replacing the ink and so on.
For fine products, the surface of the self-adhesive material must be wiped off with the exception of static brushes, electrostatic wipes, or non-woven fabrics or alcohol. According to the printing quality inspection standard, each printing press is the preliminary self-inspection unit, and the qualified products and unqualified products are strictly placed in the printing process.
When transparent adhesive materials are printed, the body color test must be carried out. Only after passing the test can it be printed.
After the printing is completed, the self-adhesive printed on Japanese Seiko ink should be pushed into the drying room. The temperature is set to 45-50°C, baked for 20-30 minutes, and then dried in the drying room; other ink types are printed. After finishing the process, you can put it in a room and dry it for 24 hours before it is dried. Otherwise, it must be placed vertically. For two-color overprinting, the color registration interval should be controlled over 30 minutes.
When collecting prints from the air baffle, ensure that the positioning edges are the same and no scratches or wrinkles occur. For the non-conforming products, use the “׆mark on the bottom side of the paper to mark the corresponding parts; Goods and non-conforming products, specify their respective quantities, and fill out the production subpena.
Fourth, knife mold production, die-cutting process
The design department makes the final product's die line pattern according to the drawing requirements, hand it to the die cutter production personnel, and after verifying it is correct, the pattern is pasted on a 5 mm thick plastic board, and the pattern outline is sawn with a sawing machine according to the die line, and the edge is required to be uniform. Sleek.
Using a die cutter, a Nissan 0.45mm x 9.5mm blade is set in the slit of the die line, and then manually cut with a sticker to check the size of the tangent, the edge is sleek or not, and the blade interface is required. There is no gap, no misplacement, and the quality inspection personnel to confirm and fill in the mold confirmation report form.
After the knife template is produced, it is glued on the blade surface with foam, and the knife blade is not damaged. Finally, the product name, production date, and producer are marked on the knife template and handed over to the die-cutting personnel.
Die-cutting personnel first check the quality of the knife template, and after confirming it is correct, number it and record it on the knife template account in time. The principle is: All the knife templates are arranged according to the customer name, and all the knife templates of each customer are arranged according to the figure number size. Can not be omitted, which makes the search knife template accurate and time-saving.
According to the production subpena, the semi-finished products must be collected from the printing process, and the quantity must be clearly identified to identify the non-conforming product of the qualified product, and whether the surface of the semi-finished product should be scratched or not, and whether the positioning is consistent with the positioning, and the mutual inspection work should be done well.
According to the production subpena and tool template ledger to find the knife template, installed on the die-cutting machine, according to the requirements of the product (half-off or full-off) to debug the pressure, the distance from large to small, and determine the die-cut positioning according to the original positioning of the printing.
During the die-cutting process, self-inspection shall be strictly performed according to the quality inspection standards for die-cutting, with a ratio of 10%, and the qualified products and non-conforming products shall be clearly distinguished. According to the counter display, 100 pieces shall be cut per die, separated by bottom paper, and the semi-finished product area shall be placed finally. Good production subpena.
The used knife template is put back to the original place. If any problem is found, fill in the rework list and return it to the mold making process. After each die-cut is completed, the date of die-cutting, number of die-cuts, and tool template shall be indicated on the tool template. Quality status. Need to drop the sticker label of crystal glue, please continue the following operations.
V. Pre-drip inspection stage
Organize personnel to the semi-manufacturing process to receive semi-finished products by production voucher, need to clear the quantity, distinguish between qualified products and non-conforming products. Check the quality of the blank side of die-cutting semi-finished products according to the quality inspection standards, distinguish the qualified and unqualified products after inspection, and label them with laminating paper to prepare for the next process; if they need to be repaired, fill in the return form and return it. Related processes.
The printing staff first obtains the corresponding screen, ink, and adhesive materials according to the production subpena and process card requirements, and performs the mutual inspection work. Specifically, the printing personnel include: 1) The received screen printing plate, whether the ink meets production subpena or process card requirements. 2 screen quality meets the quality requirements for printing; 3 check the surface quality of the edges of adhesive materials. After the inspection is correct, fix the screen and fix the net distance, and then use the positioning material for positioning. In this case, the position of the printing pattern must be determined according to the positioning frame. The three positioning pieces are located at 1/3 of each positioning edge. The size of the positioning piece is specified as 1cm x 2cm, and the position of the positioning piece at the edge of the adhesive material is marked when the original positioning is performed.
The first piece of paper is printed before the plate is printed. After the first piece of monochrome is printed, it must be confirmed by the quality inspector. Sign the "Agree to Print" on the color sample of the first product and sign it; The contrast check, found abnormal, to do appropriate adjustments, such as adding thinner, adjusting the angle of the blade, replacing the ink and so on.
For fine products, the surface of the self-adhesive material must be wiped off with the exception of static brushes, electrostatic wipes, or non-woven fabrics or alcohol. According to the printing quality inspection standard, each printing press is the preliminary self-inspection unit, and the qualified products and unqualified products are strictly placed in the printing process.
When transparent adhesive materials are printed, the body color test must be carried out. Only after passing the test can it be printed.
After the printing is completed, the self-adhesive printed on Japanese Seiko ink should be pushed into the drying room. The temperature is set to 45-50°C, baked for 20-30 minutes, and then dried in the drying room; other ink types are printed. After finishing the process, you can put it in a room and dry it for 24 hours before it is dried. Otherwise, it must be placed vertically. For two-color overprinting, the color registration interval should be controlled over 30 minutes.
When collecting prints from the air baffle, ensure that the positioning edges are the same and no scratches or wrinkles occur. For the non-conforming products, use the “׆mark on the bottom side of the paper to mark the corresponding parts; Goods and non-conforming products, specify their respective quantities, and fill out the production subpena.
Fourth, knife mold production, die-cutting process
The design department makes the final product's die line pattern according to the drawing requirements, hand it to the die cutter production personnel, and after verifying it is correct, the pattern is pasted on a 5 mm thick plastic board, and the pattern outline is sawn with a sawing machine according to the die line, and the edge is required to be uniform. Sleek.
Using a die cutter, a Nissan 0.45mm x 9.5mm blade is set in the slit of the die line, and then manually cut with a sticker to check the size of the tangent, the edge is sleek or not, and the blade interface is required. There is no gap, no misplacement, and the quality inspection personnel to confirm and fill in the mold confirmation report form.
After the knife template is produced, it is glued on the blade surface with foam, and the knife blade is not damaged. Finally, the product name, production date, and producer are marked on the knife template and handed over to the die-cutting personnel.
Die-cutting personnel first check the quality of the knife template, and after confirming it is correct, number it and record it on the knife template account in time. The principle is: All the knife templates are arranged according to the customer name, and all the knife templates of each customer are arranged according to the figure number size. Can not be omitted, which makes the search knife template accurate and time-saving.
According to the production subpena, the semi-finished products must be collected from the printing process, and the quantity must be clearly identified to identify the non-conforming product of the qualified product, and whether the surface of the semi-finished product should be scratched or not, and whether the positioning is consistent with the positioning, and the mutual inspection work should be done well.
According to the production subpena and tool template ledger to find the knife template, installed on the die-cutting machine, according to the requirements of the product (half-off or full-off) to debug the pressure, the distance from large to small, and determine the die-cut positioning according to the original positioning of the printing.
During the die-cutting process, self-inspection shall be strictly performed according to the quality inspection standards for die-cutting, with a ratio of 10%, and the qualified products and non-conforming products shall be clearly distinguished. According to the counter display, 100 pieces shall be cut per die, separated by bottom paper, and the semi-finished product area shall be placed finally. Good production subpena.
The used knife template is put back to the original place. If any problem is found, fill in the rework list and return it to the mold making process. After each die-cut is completed, the date of die-cutting, number of die-cuts, and tool template shall be indicated on the tool template. Quality status. Need to drop the sticker label of crystal glue, please continue the following operations.
V. Pre-drip inspection stage
Organize personnel to the semi-manufacturing process to receive semi-finished products by production voucher, need to clear the quantity, distinguish between qualified products and non-conforming products. Check the quality of the blank side of die-cutting semi-finished products according to the quality inspection standards, distinguish the qualified and unqualified products after inspection, and label them with laminating paper to prepare for the next process; if they need to be repaired, fill in the return form and return it. Related processes.
Seagrass Wrapped Glass,Seagrass Wrapped Tumblers,Seagrass Wrapped Glassware,Grass Wrapped Glass Cup
Shaanxi Freeway Export and Import Co.,LTD. , https://www.fw-deco.com